MSI Eureka

The quasibinary FeO-MgO system based on experimental data of [35Bow, 61Sch] and calculations [79Kau, 93 Wu]

Figure 1 from evaluation report:

Fe-Mg-O Ternary Phase Diagram Evaluation

Cite this page

Recorded Points

General Information

  • Concentration Range: Fe conc. [50-0 at.%] / Mg conc. [0-50 at.%] / O conc. [50-50 at.%]
  • Temperature: Temperature [1300-3000 °C]

Reference

About this content

  • Database name

    MSI Eureka

  • Dataset ID

    sm_msi_r_10_010323_01_full_LnkDia0

  • Copyright

    © MSI Materials Science International Services GmbH 2000

  • Chief Editor

    Günter Effenberg, Stuttgart

    effenberg@msiport.com

  • Credits

    Figure taken from MSI Eureka Evaluation Report 10.10323.1.7

    System Name: Fe-Mg-O

    Report Authors: Nathalie Lebrun and MSIT®®

    MSIT® is a registered trademark of MSI Materials Science International Services GmbH.

  • Cite this content

    Citation copied