MSI Eureka

Isothermal section of Fe-Mg-O system at 1800°C [Mw=magnesiowüstite (Fe,Mg)O] from [62Phi]

Figure 7 from evaluation report:

Fe-Mg-O Ternary Phase Diagram Evaluation

Cite this page

Recorded Points

General Information

  • Concentration Range: Mg conc. [0-100 at.%] vs. O conc. [0-100 at.%] vs. Fe conc. [0-100 at.%]
  • Temperature: 1800 °C

Reference

About this content

  • Database name

    MSI Eureka

  • Dataset ID

    sm_msi_r_10_010323_01_full_LnkDia6

  • Copyright

    © MSI Materials Science International Services GmbH 2000

  • Chief Editor

    Günter Effenberg, Stuttgart

    effenberg@msiport.com

  • Credits

    Figure taken from MSI Eureka Evaluation Report 10.10323.1.7

    System Name: Fe-Mg-O

    Report Authors: Nathalie Lebrun and MSIT®®

    MSIT® is a registered trademark of MSI Materials Science International Services GmbH.

  • Cite this content

    Citation copied