MSI Eureka

Excess integral entropies of formaton Sxs (J deg.-1mol-1) for Au-Cu-Zn alloys at 727°C; standard states solid Au, Cu, Zn

Figure 6b from evaluation report:

Au-Cu-Zn Ternary Phase Diagram Evaluation

Cite this page

Recorded Points

General Information

  • Concentration Range: Cu conc. [50-100 at.%] vs. Zn conc. [0-50 at.%] vs. Au conc. [0-50 at.%]
  • Temperature: 727 °C

Reference

About this content

  • Database name

    MSI Eureka

  • Dataset ID

    sm_msi_r_10_011081_02_full_LnkDia5

  • Copyright

    © MSI Materials Science International Services GmbH 2005

  • Chief Editor

    Günter Effenberg, Stuttgart

    effenberg@msiport.com

  • Credits

    Figure taken from MSI Eureka Evaluation Report 10.11081.2.8

    System Name: Au-Cu-Zn

    Report Authors: Nataliya Bochvar, Olga Fabrichnaya, Yurii Liberov and MSIT®®

    MSIT® is a registered trademark of MSI Materials Science International Services GmbH.

  • Cite this content

    Citation copied