Temperature-composition section Cr5Si3-C (tentative)
Figure 9 from evaluation report:
C-Cr-Si Ternary Phase Diagram Evaluation
Cite this page
General Information
- Concentration Range: Cr conc. [31.25-62.5 at.%] / Si conc. [18.75-37.5 at.%] / C conc. [50-0 at.%]
- Temperature: Temperature [1400-2050 °C]
Reference
About this content
MSI Eureka
sm_msi_r_10_011150_01_full_LnkDia7
© MSI Materials Science International Services GmbH 2010
Günter Effenberg, Stuttgart
Figure taken from MSI Eureka Evaluation Report 10.11150.1.3
System Name: C-Cr-Si
Report Authors: Nathalie Lebrun, Pierre Perrot, An Serbruyns, Jean-Claude Tedenac and MSIT®®
MSIT® is a registered trademark of MSI Materials Science International Services GmbH.