MSI Eureka

The MoO3-tau5,MoFeO4 quasibinary system

Figure 2 from evaluation report:

Fe-Mo-O Ternary Phase Diagram Evaluation

Cite this page

Recorded Points

General Information

  • Concentration Range: Mo conc. [25-16.65 at.%] / Fe conc. [0-16.65 at.%] / O conc. [75-66.7 at.%]
  • Temperature: Temperature [600-1100 °C]

Reference

About this content

  • Database name

    MSI Eureka

  • Dataset ID

    sm_msi_r_10_012440_01_full_LnkDia1

  • Copyright

    © MSI Materials Science International Services GmbH 2008

  • Chief Editor

    Günter Effenberg, Stuttgart

    effenberg@msiport.com

  • Credits

    Figure taken from MSI Eureka Evaluation Report 10.12440.1.7

    System Name: Fe-Mo-O

    Report Authors: Pierre Perrot and MSIT®®

    MSIT® is a registered trademark of MSI Materials Science International Services GmbH.

  • Cite this content

    Citation copied