Isothermal section at 400°C
Figure 1 from evaluation report:
Cu-La-Ni Ternary Phase Diagram Evaluation
Cite this page
General Information
- Concentration Range: Ni conc. [0-100 at.%] vs. Cu conc. [0-100 at.%] vs. La conc. [0-100 at.%]
- Temperature: 400 °C
Reference
About this content
MSI Eureka
sm_msi_r_10_013710_01_full_LnkDia0
© MSI Materials Science International Services GmbH 2006
Günter Effenberg, Stuttgart
Figure taken from MSI Eureka Evaluation Report 10.13710.1.2
System Name: Cu-La-Ni
Report Authors: Gautam Ghosh and MSIT®®
MSIT® is a registered trademark of MSI Materials Science International Services GmbH.