Partial isotherm at 450°C of the (gMn,Ni,Cu) solvus surface and phase boundaries of the ordered phase
Figure 3 from evaluation report:
Cu-Mn-Ni Ternary Phase Diagram Evaluation
Cite this page
General Information
- Concentration Range: Ni conc. [0-60 at.%] vs. Cu conc. [40-100 at.%] vs. Mn conc. [0-60 at.%]
- Temperature: 450 °C
Reference
About this content
MSI Eureka
sm_msi_r_10_015881_02_full_LnkDia2
© MSI Materials Science International Services GmbH 2016
Günter Effenberg, Stuttgart
Figure taken from MSI Eureka Evaluation Report 10.15881.2.9
System Name: Cu-Mn-Ni
Report Authors: Andy Watson, Sigrid Wagner, Evgeniya Lysova and Lazar Rokhlin, updated by Andy Watson, updated by Liya Dreval and MSIT®®
MSIT® is a registered trademark of MSI Materials Science International Services GmbH.