Isothermal section at 500°C
Figure 4 from evaluation report:
Ag-Cd-Cu Ternary Phase Diagram Evaluation
Cite this page
General Information
- Concentration Range: Ag conc. [0-100 at.%] vs. Cd conc. [0-100 at.%] vs. Cu conc. [0-100 at.%]
- Temperature: 500 °C
Reference
About this content
MSI Eureka
sm_msi_r_10_016018_02_full_LnkDia2
© MSI Materials Science International Services GmbH 2005
Günter Effenberg, Stuttgart
Figure taken from MSI Eureka Evaluation Report 10.16018.2.4
System Name: Ag-Cd-Cu
Report Authors: Guenter Effenberg updated by Nele Moelans, Pierre Perrot, Nathalie Lebrun and MSIT®®
MSIT® is a registered trademark of MSI Materials Science International Services GmbH.
Cite this content