MSI Eureka

Enthalpies of formation of alloys calculated from empirical potentials/expressed in eV, after [2010Dai].

Figure 3 from evaluation report:

Mo-Ta-W Ternary Phase Diagram Evaluation

Cite this page

Recorded Points

General Information

  • Concentration Range: W conc. [0-100 at.%] vs. Mo conc. [0-100 at.%] vs. Ta conc. [0-100 at.%]

Reference

About this content

  • Database name

    MSI Eureka

  • Dataset ID

    sm_msi_r_10_018990_01_full_LnkDia2

  • Copyright

    © MSI Materials Science International Services GmbH 2015

  • Chief Editor

    Günter Effenberg, Stuttgart

    effenberg@msiport.com

  • Credits

    Figure taken from MSI Eureka Evaluation Report 10.18990.1.3

    System Name: Mo-Ta-W

    Report Authors: Jean-Claude Tedenac, Alina Makudera, Vladimir Cheverikin, Gautam Ghosh and MSIT®®

    MSIT® is a registered trademark of MSI Materials Science International Services GmbH.

  • Cite this content

    Citation copied