MSI Eureka

Schematic partial isothermal section at 400°C based on [84Daa]

Figure 1 from evaluation report:

Au-Hg-Mg Ternary Phase Diagram Evaluation

Cite this page

Recorded Points

General Information

  • Concentration Range: Au conc. [0-50 at.%] vs. Hg conc. [0-50 at.%] vs. Mg conc. [50-100 at.%]
  • Temperature: 400 °C

Reference

About this content

  • Database name

    MSI Eureka

  • Dataset ID

    sm_msi_r_10_020391_01_full_LnkDia0

  • Copyright

    © MSI Materials Science International Services GmbH 1995

  • Chief Editor

    Günter Effenberg, Stuttgart

    effenberg@msiport.com

  • Credits

    Figure taken from MSI Eureka Evaluation Report 10.20391.1.8

    System Name: Au-Hg-Mg

    Report Authors: Nataliya R. Bochvar and Yurii P. Liberov and MSIT®®

    MSIT® is a registered trademark of MSI Materials Science International Services GmbH.

  • Cite this content

    Citation copied