Partial isothermal section at 300 °C
Figure 1 from evaluation report:
Ca-Mg-Zn Ternary Phase Diagram Evaluation
Cite this page
General Information
- Concentration Range: Zn conc. [0-100 at.%] vs. Ca conc. [0-100 at.%] vs. Mg conc. [0-100 at.%]
- Temperature: 300 °C
Reference
About this content
MSI Eureka
sm_msi_r_10_020521_01_full_LnkDia0
© MSI Materials Science International Services GmbH 2000
Günter Effenberg, Stuttgart
Figure taken from MSI Eureka Evaluation Report 10.20521.1.6
System Name: Ca-Mg-Zn
Report Authors: Evgeniya Lysova, Lazar Rokhlin and Andriy Grytsiv and MSIT®®
MSIT® is a registered trademark of MSI Materials Science International Services GmbH.
Cite this content