Isothermal section at 400°C [74Dri1]
Figure 4 from evaluation report:
Mg-Nd-Zn Ternary Phase Diagram Evaluation
Cite this page
General Information
- Concentration Range: Mg conc. [95-100 at.%] vs. Zn conc. [0-5 at.%] vs. Nd conc. [0-5 at.%]
- Temperature: 400 °C
Reference
About this content
MSI Eureka
sm_msi_r_10_021031_02_full_LnkDia2
© MSI Materials Science International Services GmbH 2001
Günter Effenberg, Stuttgart
Figure taken from MSI Eureka Evaluation Report 10.21031.2.1
System Name: Mg-Nd-Zn
Report Authors: Geert Davignon, Mauro Giovannini, Joachim Gröbner, Gregory Haidemenopoulos, Hans Jürgen Seifert and MSIT®®