100 result(s) using Focused Search for substance: consolidated al3zr
If you didn't find what you were looking for, see more results.
Properties:
isothermal section
100 result(s) using Focused Search for substance: consolidated al3zr
If you didn't find what you were looking for, see more results.
  1. Inorganic Solid Phases

    Al-Mg-Zr Isothermal Section of Ternary Phase Diagram

    • Temperature: 800 °C (1073 K); Partial composition: Al1.4Mg98.6-Mg-Mg98.3Zr1.7, Mg-rich corner; Investigation: experimental; schematic
  2. Inorganic Solid Phases

    Al-Fe-Zr Isothermal Section of Ternary Phase Diagram

    • Temperature: 500 °C (773 K); Partial composition: Al-Al75Fe25-Al75Zr25, 75-100 at.% Al; Investigation: experimental; detailed
  3. Inorganic Solid Phases

    Al-Sc-Zr Isothermal Section of Ternary Phase Diagram

    • Temperature: 600 °C (873 K); Partial composition: Al-Al98.8Sc1.2-Al98.8Zr1.2, 98.8-100 at.% Al; Investigation: experimental; detailed
  4. Inorganic Solid Phases

    Al-Sc-Zr Isothermal Section of Ternary Phase Diagram

    • Temperature: 550 °C (823 K); Partial composition: Al-Al98.8Sc1.2-Al98.8Zr1.2, 98.8-100 at.% Al; Investigation: experimental; detailed
  5. Inorganic Solid Phases

    Al-Cr-Zr Isothermal Section of Ternary Phase Diagram

    • Temperature: 620 °C (893 K); Partial composition: Al-Al91.5Cr8.5-Al90Zr10, Al-rich corner; Investigation: calculated; detailed
  6. Inorganic Solid Phases

    Al-Cr-Zr Isothermal Section of Ternary Phase Diagram

    • Temperature: 450 °C (723 K); Partial composition: Al-Al91.5Cr8.5-Al90Zr10, Al-rich corner; Investigation: calculated; detailed
  7. Inorganic Solid Phases

    Al-Mg-Zr Isothermal Section of Ternary Phase Diagram

    • Temperature: 400 °C (673 K); Partial composition: Al-Al80Mg20-Al80Mg19.3Zr0.7, 0-5 wt.% Zr; Investigation: experimental; detailed
  8. Inorganic Solid Phases

    Al-Si-Zr Isothermal Section of Ternary Phase Diagram

    • Temperature: 525 °C (798 K); Partial composition: Al-Al98Si2-Al98Zr2, 98-100 at.% Al; Investigation: experimental; detailed
  9. Inorganic Solid Phases

    Al-Si-Zr Isothermal Section of Ternary Phase Diagram

    • Temperature: 500 °C (773 K); Partial composition: Al-Al97.7Si2.3-Al97.7Zr2.3, 97.7-100 at.% Al; Investigation: experimental; detailed
  10. Inorganic Solid Phases

    Al-Si-Zr Isothermal Section of Ternary Phase Diagram

    • Temperature: 400 °C (673 K); Partial composition: Al-Al99Si1-Al99Zr1, 99-100 at.% Al; Investigation: experimental; detailed
  11. Inorganic Solid Phases

    Al-Cr-Zr Isothermal Section of Ternary Phase Diagram

    • Temperature: 620 °C (893 K); Partial composition: Al-Al99.35Cr0.65-Al99.35Zr0.65, 99.35-100 at.% Al; Investigation: experimental; detailed
  12. Inorganic Solid Phases

    Al-Sc-Zr Isothermal Section of Ternary Phase Diagram

    • Temperature: 550 °C (823 K); Partial composition: Al-Al99.4Sc0.6-Al99.4Sc0.48Zr0.12-Al99.67Zr0.33, Al-rich corner; Investigation: experimental; detailed
  13. Inorganic Solid Phases

    Al-Sc-Zr Isothermal Section of Ternary Phase Diagram

    • Temperature: 600 °C (873 K); Partial composition: Al-Al99.4Sc0.6-Al99.65Zr0.35, Al-rich corner; Investigation: experimental; detailed
  14. Inorganic Solid Phases

    Al-U-Zr Isothermal Section of Ternary Phase Diagram

    • Temperature: 1300 °C (1573 K); Partial composition: Al-UAl2-ZrAl2, 66.7-100 at.% Al; Investigation: experimental; detailed
  15. Inorganic Solid Phases

    Al-U-Zr Isothermal Section of Ternary Phase Diagram

    • Temperature: 1300 °C (1573 K); Partial composition: Al-UAl2-ZrAl2, 66.7-100 at.% Al; Investigation: experimental; detailed
  16. Inorganic Solid Phases

    Al-Gd-Zr Isothermal Section of Ternary Phase Diagram

    • Temperature: 497 °C (770 K); Partial composition: Al-Al66.7Gd33.3-Al66.7Zr33.3, 66.7-100 at.% Al; Investigation: experimental; detailed
  17. Inorganic Solid Phases

    Al-Lu-Zr Isothermal Section of Ternary Phase Diagram

    • Temperature: 497 °C (770 K); Partial composition: Al-Al66.7Lu33.3-Al66.7Zr33.3, 66.7-100 at.% Al; Investigation: experimental; detailed
  18. Inorganic Solid Phases

    Al-Ni-Zr Isothermal Section of Ternary Phase Diagram

    • Temperature: 25 °C (298 K); Partial composition: Al-Al60Ni40-Al60Ni15Zr25-Al75Zr25, 60-100 at.% Al; Investigation: experimental; detailed
  19. Inorganic Solid Phases

    Al-Cu-Zr Isothermal Section of Ternary Phase Diagram

    • Temperature: 400 °C (673 K); Partial composition: Al-CuAl2-Al66Cu12Zr22-ZrAl2, Al-rich corner; Investigation: experimental; detailed
  20. Inorganic Solid Phases

    Al-Cu-Zr Isothermal Section of Ternary Phase Diagram

    • Temperature: 400 °C (673 K); Partial composition: Al-CuAl2-Al62.5Cu12.5Zr25-ZrAl2, 62-100 at.% Al; Investigation: experimental; detailed
Page is not a valid page number. Please enter a number between 1 and 5 of 5