14 result(s) using Focused Search for substance: consolidated silver gallium diselenide
If you didn't find what you were looking for, see more results.
Properties:
phase diagram
14 result(s) using Focused Search for substance: consolidated silver gallium diselenide
If you didn't find what you were looking for, see more results.
Properties: phase diagram
  1. Inorganic Solid Phases

    Ag-Ga-Se Vertical Section of Ternary Phase Diagram

    • Temperature: 600…900 °C (873…1173 K); Partial composition: Ag27.5Ga27.5Se45-Ag22.5Ga22.5Se55, AgGa-Se (partial); Investigation: experimental; detailed
  2. Inorganic Solid Phases

    Ag-Ga-Se Vertical Section of Ternary Phase Diagram

    • Temperature: 0…1000 °C (273…1273 K); Partial composition: AgGaSe2-Se; Investigation: experimental; detailed
  3. Inorganic Solid Phases

    Ag-Ga-Se Vertical Section of Ternary Phase Diagram

    • Temperature: 600…900 °C (873…1173 K); Partial composition: Ag30Ga30Se40-Ag20Ga20Se60, Ag/Ga 1/1; Investigation: experimental; schematic
  4. Landolt-Börnstein

    Silver gallium selenide (AgGaSe2) crystal structure, lattice parameters, thermal expasion, melting point

    This document is part of Subvolume E ‘Ternary Compounds, Organic Semiconductors’ of Volume 41 ‘Semiconductors’ of Landolt-Börnstein - Group III Condensed Matter.
  5. Inorganic Solid Phases

    Ag-Ga-Se Vertical Section of Ternary Phase Diagram

    • Temperature: 350…950 °C (623…1223 K); Partial composition: Ag16.3Ga30.2Se53.5-Ag28.2Ga23.1Se48.7, Ag2Se-Ga2Se3 (partial); Investigation: experimental; detailed
  6. Inorganic Solid Phases

    Ag-Ga-Se Vertical Section of Ternary Phase Diagram

    • Temperature: 600…900 °C (873…1173 K); Partial composition: AgGaSe2-Ag2Se; Investigation: experimental; detailed
  7. Inorganic Solid Phases

    Ag-Ga-Se Vertical Section of Ternary Phase Diagram

    • Temperature: 600…1050 °C (873…1323 K); Partial composition: Ag2Se-Ga2Se3; Investigation: experimental; detailed
  8. Inorganic Solid Phases

    Ag-Ga-Se Isothermal Section of Ternary Phase Diagram

    • Temperature: 177 °C (450 K); Partial composition: Ag2Se-Ga2Se3-Se; Investigation: experimental; detailed
  9. Inorganic Solid Phases

    Ag-Ga-Se Vertical Section of Ternary Phase Diagram

    • Temperature: 600…1050 °C (873…1323 K); Partial composition: Ag2Se-Ga2Se3; Investigation: experimental; detailed
  10. Inorganic Solid Phases

    Ag-Ga-Se Vertical Section of Ternary Phase Diagram

    • Temperature: 0…1050 °C (273…1323 K); Partial composition: Ag2Se-Ga2Se3; Investigation: experimental; detailed
  11. MSI Eureka

    Ag-Ga-Se Ternary Phase Diagram Evaluation

    • This report for the ternary system Ag-Ga-Se discusses pseudobinary section, solid phases, and invariant equilibria.
  12. Inorganic Solid Phases

    Ag-Ga-Se Liquidus Projection of Ternary Phase Diagram

    • Partial composition: Ag2Se-Ga2Se3-Se; Investigation: experimental; detailed
  13. MSI Eureka

    Ag-Ga-Te Ternary Phase Diagram Evaluation

    • This report for the ternary system Ag-Ga-Te discusses pseudobinary sections, and solid phases.
  14. Landolt-Börnstein

    AgCuCdFeMnSSnZn - AgGePrS

    This document is part of Subvolume B1 ‘Sulfides, Selenides, Tellurides (Part 1)’ of Volume 14 ‘Structure Data of Elements and Intermetallic Phases’ of Landolt-Börnstein - Group III Condensed Matter.